Steel Library/Shirogami #3 / White Steel #3
Carbon Steel
Intermediate
Mid-range

Shirogami #3 / White Steel #3

Heat Treatment Specifications

Austenitizing

Temperature780°C(1436°F)
Soak Time10 minutes

Tempering

Temperature180°C(356°F)
Time60 minutes
Cycles1x

Quench Medium

water

Target Hardness

60 - 62 HRC

Performance Characteristics

Toughness7.5/10
Edge Retention6/10
Corrosion Resistance0.5/10
Ease of Sharpening9.5/10
Overall Score23.5/40