Steel Library/K720 / O2
Tool Steel
Intermediate
Mid-range

K720 / O2

Heat Treatment Specifications

Austenitizing

Temperature820°C(1508°F)
Soak Time5 minutes

Tempering

Temperature200°C(392°F)
Time90 minutes
Cycles2x

Quench Medium

oil

Target Hardness

58 - 60 HRC

Performance Characteristics

Toughness6.5/10
Edge Retention5.5/10
Corrosion Resistance1/10
Ease of Sharpening8.5/10
Overall Score21.5/40

Interesting Facts

  • 1Böhler designation for AISI O2 oil-hardening tool steel
  • 2Popular in European bushcraft knife scene
  • 3Mora has used O2/K720 in Classic line for decades
  • 4Easy to heat treat - good for beginner bladesmiths
  • 51.1% carbon, manganese for hardenability

Famous Uses

Mora Classic knives
Bushcraft knives
Woodworking tools

Best For

Light-medium use knives
Working blades
Outdoor knives

Similar Steels

O1

American equivalent

80CrV2

Modern alternative

Not Recommended For

  • Wet environments
  • Budget projects

Expert Tips

  • 1Oil hardening required
  • 263-65 HRC achievable
  • 3Good balance of properties
  • 4Needs rust protection

Track Your K720 / O2 Heat Treats

Start logging your heat treatment cycles with K720 / O2. Track what works, compare results, and repeat your best blades.

© 2026 BladesmithHub. All rights reserved.