Steel Library/10Cr15CoMoV
Stainless Steel
Intermediate
Mid-range

10Cr15CoMoV

Heat Treatment Specifications

Austenitizing

Temperature1080°C(1976°F)
Soak Time20 minutes

Tempering

Temperature200°C(392°F)
Time120 minutes
Cycles2x

Quench Medium

oil

Target Hardness

59 - 62 HRC

Performance Characteristics

Toughness7/10
Edge Retention7.5/10
Corrosion Resistance7.5/10
Ease of Sharpening6.5/10
Overall Score28.5/40

Interesting Facts

  • 1Chinese powder metallurgy stainless
  • 2Contains cobalt for improved properties
  • 31.0% carbon, 15% chromium + Co, Mo, V
  • 4Similar performance tier to VG-10
  • 5Used in premium Chinese knife production
  • 6Represents China's high-end steel capabilities

Famous Uses

Chinese premium kitchen knives
High-end Chinese folders

Best For

Premium kitchen knives
Chef's knives
Folding knives
Survival knives

Similar Steels

Not Recommended For

  • Budget projects
  • Beginners
  • Rough work

Expert Tips

  • 1Cobalt intensifies hardness
  • 2Red hot hardness property
  • 3Careful heat treatment required
  • 4Popular VG-10 equivalent

Track Your 10Cr15CoMoV Heat Treats

Start logging your heat treatment cycles with 10Cr15CoMoV. Track what works, compare results, and repeat your best blades.

© 2026 BladesmithHub. All rights reserved.